Saturable absorber in transmission mode for laser mode-locking,
for instance in a fiber ring laser
-> see information "transmission loss of fiber coupled SA" (pdf),
flyer: "SA - saturable absorber" (pdf)
• Wavelength λ = 2800 nm
• Absorptance A = 10 %
• Relaxation time τ = 10 ps
• Substrate thickness = 625 µm
• Data sheet (pdf)
• Mounting & price table
• Order form
• x = 5.0-0
• Single chip, unmounted
• Chip area 5.0 mm x 5.0 mm
• Chip thickness 625 µm, both sides AR coated
• Data sheet (pdf)
• Price: 699.- €/pc
• x = 1.0b-0
• Batch of 4 unmounted chips
• Chip area 1.0 mm x 1.0 mm
• Chip thickness 150 µm, for fiber laser butt coupling,
• Data sheet (pdf)
• Price: 699.- €/batch
• x = 1.3b-0
• Batch of 4 unmounted chips
• Chip area 1.3 mm x 1.3 mm
• Chip thickness 150 µm, for fiber laser butt coupling,
• Data sheet (pdf)
• Price: 699.- €/batch
• x = 5.0-12.7g-c / 5.0-12.7g-e
• Chip area 5.0 mm x 5.0 mm
• Chip thickness 625 µm, both sides AR coated
• Glued on a copper heat sink with 12.7 mm diameter and 4 mm hole
• Center mounted : x = 5.0-12.7g-c
• Edge mounted : x = 5.0-12.7g-e
• Data sheet (pdf)
• Price: 786.- €/pc
• x = 5.0-25.0g-c / 5.0-25.0g-e
• Chip area 5.0 mm x 5.0 mm
• Chip thickness 625 µm, both sides AR coated
• Glued on a copper heat sink with 25.0 mm diameter and 4 mm hole
• Center mounted : x = 5.0-25.0g-c
• Edge mounted : x = 5.0-25.0g-e
• Data sheet (pdf)
• Price: 786.- €/pc
• x = 5.0-25.4g-c / 5.0-25.4g-e
• Chip area 5.0 mm x 5.0 mm
• Chip thickness 625 µm, both sides AR coated
• Glued on a copper heat sink with 25.4 mm diameter and 4 mm hole
• Center mounted : x = 5.0-25.4g-c
• Edge mounted : x = 5.0-25.4g-e
• Data sheet (pdf)
• Price: 786.- €/pc